>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by dcaster@krl.org on August 4, 2007, 11:42 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Mouse on August 4, 2007, 11:48 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Larry Jaques on August 4, 2007, 11:52 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Gunner Asch on August 5, 2007, 4:49 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
bench belt and disc sander March 28, 2006, 1:39 am
Belt sander: Smoke escape! February 17, 2008, 7:24 pm
making wheels for belt sander; bearings, rubber coating? April 4, 2006, 12:11 am
Sanding belt question... July 19, 2006, 10:44 pm
www.BeltPolice.Com Belt Holsters Accessories Bargains Leather DUTY POLICE Law Enforcement BELT August 14, 2007, 11:34 pm
www.BeltPolice.Com Belt Holsters Accessories Bargains Leather DUTY POLICE Law Enforcement BELT August 14, 2007, 11:36 pm
12" disc sander December 13, 2006, 5:13 pm
need 2 x 32" belts for sander September 9, 2007, 5:57 pm
Performax benchtop sander June 3, 2007, 6:39 pm
HF Inline Sander Mods September 10, 2007, 12:15 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap