Subject Author Date
20Ft Shipping Container to Machine Shop Conversion Brent 06-13-2007
Posted by Harold and Susan Vordos on June 19, 2007, 1:59 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on June 19, 2007, 4:02 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by DoN. Nichols on June 18, 2007, 8:03 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Al Patrick on June 18, 2007, 9:06 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Larry Jaques on June 18, 2007, 9:37 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Steel cargo container shop shipping. May 9, 2006, 12:01 pm
Moving a 20' shipping container Results July 29, 2007, 2:00 pm
Moving a 20' shipping container 20 feet by hand July 4, 2007, 2:09 pm
how to do these w/o machine shop (or even with, for some)? August 6, 2006, 9:31 am
Machine shop in or near SF? April 30, 2007, 8:55 pm
Little Machine Shop! September 6, 2007, 6:49 pm
Re: MACHINE SHOP STARTUP July 5, 2006, 9:40 pm
setting up a machine shop December 11, 2006, 2:40 am