>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by DoN. Nichols on April 23, 2007, 1:11 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Trevor Jones on April 23, 2007, 8:07 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Dave on April 23, 2007, 3:18 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Trevor Jones on April 23, 2007, 6:26 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Flather shaper info April 23, 2007, 9:42 am
25" Smith & Mills shaper info January 23, 2007, 9:15 am
20 inch Steptoe Shaper info needed. January 18, 2007, 10:59 pm
OT-Computer nerds request November 4, 2006, 3:36 am
Metal shavings request June 30, 2007, 1:28 pm
i am wistfully weak, so I request you August 12, 2007, 6:26 pm
Electric motor wiring request July 9, 2006, 12:48 pm
Aluminum bronze and Copper help request August 18, 2006, 5:01 pm
OT request for post from years back November 3, 2006, 2:22 pm
Request for source to buy a low quantity of waylube oil from November 27, 2006, 10:11 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap