Posted by Wild Bill on January 18, 2007, 7:24 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by buffalo on January 18, 2007, 9:59 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Unknown on January 19, 2007, 7:13 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by buffalo on January 19, 2007, 4:05 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Andy Dingley on January 19, 2007, 4:16 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Re: Brass alloys and copper green crud January 20, 2007, 10:44 am
copper to brass April 1, 2006, 6:02 am
Making machine screw threads vibration proof in copper-to-brass connection July 29, 2006, 1:58 am
Titanium Alloys? May 7, 2008, 10:08 am
How to cut very hard cast alloys? July 14, 2006, 5:13 am
European steel alloys August 4, 2006, 9:43 am
using Low melting temp alloys for dies for wax models April 5, 2007, 7:07 pm
OT: Green Washing December 7, 2007, 12:09 pm
Green LEDS? Who needed em? April 17, 2007, 12:17 am
Taps in green coating October 11, 2007, 10:18 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap