Cratex rubberized "grinding" wheel

General Metalworking - All aspects of working with metal. 

Bookmark this page:  YahooMyWeb Yahoo!  Google Google  Windows Live Favorites Windows Live  del.icio.us del.icio.us  digg digg  Add to Netscape Netscape
Subject Author Date
Cratex rubberized "grinding" wheel Bob Engelhardt 09-01-2007
Posted by Bob Engelhardt on September 1, 2007, 10:38 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Mark F on September 2, 2007, 12:24 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Wes on September 2, 2007, 2:02 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Martin H. Eastburn on September 2, 2007, 10:01 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Gunner Asch on September 3, 2007, 12:07 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Grinding wheel safety October 4, 2006, 8:41 pm
Grinding-wheel safety May 25, 2007, 1:10 pm
Grinding wheel recommendation, please? October 25, 2007, 7:50 pm
Question on mounting a grinding wheel October 12, 2006, 8:28 pm
grinding wheel clogged with aluminum January 16, 2007, 11:55 am
Grinding wheel peripheral speed question July 23, 2007, 4:31 pm
What diamond/green wheel for side grinding on my bench grinder? November 26, 2008, 12:01 pm
Herbert No2 grinding jig September 23, 2006, 11:55 pm
Tool grinding May 3, 2007, 11:46 pm
grinding finish July 11, 2007, 8:56 am

Contact Us | Privacy Policy