Decent cut-off tool Louis Ohland 12-09-2007
Posted by Louis Ohland on December 9, 2007, 7:24 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Harold and Susan Vordos on December 9, 2007, 7:42 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Louis Ohland on December 9, 2007, 7:52 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Harold and Susan Vordos on December 9, 2007, 11:57 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Grant Erwin on December 9, 2007, 8:10 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Grinding a blank lathe tool for parting or cutoff December 8, 2008, 2:48 pm
cutoff bandsaws March 19, 2007, 2:26 pm
Hilti DS HS 80 Gas cutoff saw May 19, 2007, 11:54 am
Cutoff Inserts & Blades? November 4, 2006, 5:13 pm
Abrasive Cutoff Saw Issues November 26, 2008, 5:33 pm
update on reclamation of old 16" abrasive cutoff saw May 4, 2006, 12:35 am
ForSale: Misc. cutoff blades January 17, 2008, 11:43 pm
welding rods from CHINA - anybody ever use one (besides gunner?). also cutoff wheels... April 29, 2006, 9:59 am
Decent Welding Rod?? May 24, 2007, 11:08 am
decent impact wrench? May 9, 2007, 1:29 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap