Posted by Proctologically Violated©® on November 20, 2006, 7:58 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Howard R Garner on November 20, 2006, 8:33 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Proctologically Violated©® on November 20, 2006, 8:36 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Andrew Mawson on November 21, 2006, 3:11 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Leo Lichtman on November 20, 2006, 4:29 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Gold Refining Community February 27, 2007, 10:43 am
Gold refining forum March 4, 2007, 6:06 pm
Gold Refining Forum (community) March 22, 2007, 8:33 pm
gold colours? December 21, 2006, 11:06 am
Why is gold yellow? December 27, 2006, 11:18 am
(((((( - We Buy Scrap Gold - )))))) June 17, 2007, 10:40 pm
gold leaf August 15, 2007, 11:56 am
The Malleability of Gold November 29, 2007, 10:41 am
Gold - yes, it's metal March 19, 2008, 2:34 pm
dental gold? August 5, 2008, 6:11 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap