Engraving a degree scale grice 03-21-2007
Posted by whit3rd on March 21, 2007, 4:33 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by John on March 21, 2007, 9:26 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on March 21, 2007, 5:18 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by kfvorwerk@gmail.com on March 22, 2007, 7:36 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on March 22, 2007, 10:23 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Engraving a degree scale December 4, 2007, 11:12 am
CNC Engraving from Halftones March 9, 2007, 10:25 pm
Engraving tools - angle October 12, 2006, 5:22 am
Milling/Engraving Horseshoes? May 31, 2007, 1:05 am
Paint filling for engraving on ABS plastic? March 3, 2008, 4:37 pm
Degree symbol =?ISO-8859-1?Q?=B0?= December 22, 2007, 1:28 pm
Re: 45 degree angle drive? March 7, 2006, 7:04 pm
Metal Engraving chasing vintage engravers manual 1908 FA May 16, 2006, 6:55 pm
Source for 82 Degree Countersinks for Mircostops? April 29, 2007, 10:29 am
90 Degree joints, square tube steel April 20, 2006, 12:42 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap