Find three phase "wild" leg

General Metalworking - All aspects of working with metal. 

Bookmark this page:  YahooMyWeb Yahoo!  Google Google  Windows Live Favorites Windows Live  del.icio.us del.icio.us  digg digg  Add to Netscape Netscape
Subject Author Date
Find three phase "wild" leg Karl Townsend 11-20-2006
Posted by Karl Townsend on November 20, 2006, 8:04 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Pete C. on November 20, 2006, 8:56 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Pete C. on November 20, 2006, 9:07 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Ignoramus25600 on November 20, 2006, 9:25 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on November 21, 2006, 6:50 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
rcmp gone wild February 29, 2008, 5:25 pm
it can seriously suck up to sympathetic wild workstations August 12, 2007, 11:43 pm
21 of the Strangest Cars I Have Ever Seen (Wild Metalworking) October 1, 2008, 12:43 am
profit-motive question: single phase adapter for 3-phase motor drives October 4, 2007, 5:30 pm
FA: cool (and qute old) phase sequence indicator (for testing three phase power) October 21, 2006, 1:56 am
Replacement lathe tool posts Phase II, Phase 2 and HF 39083 comparison January 7, 2007, 10:46 am
[ADV] Phase-A-Matic Phase Converter on EBay Item # 230127447458 May 10, 2007, 5:42 pm
Rotary phase converter versus trying to run a VMC straight from single phase February 19, 2008, 12:44 am
Is it practical for a RPC to generate 440 volt 3-phase from 220 single phase? November 27, 2006, 10:03 pm
3 phase 200V, on (nominal 240) rotary phase converter December 28, 2007, 4:27 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap