Posted by SteveF on December 29, 2006, 12:51 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Larry Jaques on December 28, 2006, 12:13 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Tony on December 27, 2006, 8:50 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Steve Austin on December 29, 2006, 4:53 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Larry Jaques on December 29, 2006, 10:28 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
win a ford f-150 sweepstakes May 17, 2007, 4:06 am
OT - Ford fan clutch November 5, 2007, 12:05 pm
diesel in 93 Ford gas November 26, 2007, 1:59 pm
Henry Ford March 10, 2008, 12:53 am
Ford Escape August 5, 2008, 10:54 pm
Tractors, Ford 8N & similar September 26, 2006, 4:46 pm
what is this part (somewhat OT, think it fits an old Ford) December 10, 2006, 3:39 pm
Ford F-250 common problems December 21, 2006, 2:02 pm
Ford E350 Extended Van July 1, 2007, 10:51 pm
What should I do? Ford Ranger avaible to me July 13, 2007, 1:05 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap