Green low-friction coating in Clausing Varidrives Joseph Gwinn 01-20-2008
Posted by Joseph Gwinn on January 20, 2008, 10:31 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Wes on January 20, 2008, 1:13 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Taps in green coating October 11, 2007, 10:18 am
OT: Green Washing December 7, 2007, 12:09 pm
DIY powder coating? February 9, 2007, 1:40 pm
Green LEDS? Who needed em? April 17, 2007, 12:17 am
tiny green spot April 7, 2006, 2:30 am
Give your FOREX the green light. March 18, 2008, 12:32 pm
Re: Tool coating technologies September 14, 2006, 9:38 am
removing powder coating? October 9, 2006, 9:47 pm
HF powder coating system November 12, 2006, 8:58 pm
AlCrN for tool coating March 27, 2006, 8:02 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap