Posted by michael gray on February 27, 2007, 12:08 pm
Please log in for more thread options
>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore
Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.
Cheers
--
Jeff R.
|
|
Posted by Wild Bill on February 28, 2007, 8:01 am
Please log in for more thread options
>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore
Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.
Cheers
--
Jeff R.
|
|
Posted by Bernd on February 27, 2007, 9:47 am
Please log in for more thread options
>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore
Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.
Cheers
--
Jeff R.
|
|
Posted by trg-s338 on February 27, 2007, 5:10 pm
Please log in for more thread options
>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore
Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.
Cheers
--
Jeff R.
|
|
Posted by trg-s338 on February 27, 2007, 5:14 pm
Please log in for more thread options
>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore
Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.
Cheers
--
Jeff R.
|
| Similar Threads | Posted | | Circular saws , worm drive , hypoid gear | December 6, 2006, 3:16 pm |
| Cheap gears | January 4, 2007, 9:19 pm |
| Cheap gears | January 4, 2007, 10:30 pm |
| Books on gears | October 1, 2007, 12:14 pm |
| Types of Gears | November 7, 2007, 5:51 am |
| Pictures of Gears | November 8, 2007, 11:43 am |
| Helical Gears | January 2, 2008, 5:38 pm |
| worm gears | March 28, 2006, 9:40 pm |
| Types of Gears | February 18, 2008, 11:05 pm |
| Brass Gears. Need some made. | October 13, 2006, 12:56 am |
|
|
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore