>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Pete C. on October 4, 2007, 9:51 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on October 4, 2007, 1:23 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Pete C. on October 4, 2007, 2:11 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on October 4, 2007, 4:00 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
welded wire mesh project November 20, 2006, 2:57 pm
Straightening Rolled Welded Wire Mesh September 16, 2008, 9:56 pm
Need wire mesh rounds in Stainless Steel October 27, 2008, 9:27 pm
FS: Heavy Metal Cabinets with Adjustable Shelves - Dallas, TX March 26, 2007, 1:16 pm
My Posts November 10, 2007, 10:32 am
My posts October 6, 2008, 12:15 am
[OT] All the political posts here. October 20, 2006, 4:00 am
no posts? test December 13, 2006, 7:27 am
Help with small mesh screen / filter ID April 24, 2007, 7:54 am
Introducing The Hz2.1 Portable Hot Stamp Wire Marker to Meet Industry's Need for Flexible, Cost-effective Wire Marking April 30, 2007, 4:13 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap