Module & Diametral threads? Eric R Snow 01-11-2007
Posted by Eric R Snow on January 11, 2007, 4:21 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Trevor Jones on January 12, 2007, 8:35 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Eric R Snow on January 12, 2007, 10:52 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Nick Mueller on January 12, 2007, 9:45 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Eric R Snow on January 12, 2007, 7:04 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
5/16-27 threads August 8, 2008, 3:03 pm
More on odd threads.... September 26, 2008, 8:28 pm
Help with lathe threads April 30, 2007, 11:57 pm
Threads question August 14, 2007, 2:12 am
'hand' die cut threads ; 1/2" NC .... ??how?? April 12, 2006, 10:52 pm
cutting npt threads March 23, 2006, 6:34 am
Threads off axis June 28, 2008, 10:10 pm
Need advice... have to cut 1/4 - 20 threads in 1/2" aluminum March 24, 2007, 7:39 pm
Repairing external threads April 23, 2007, 7:33 pm
Strength of aluminum threads April 25, 2007, 12:25 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap