>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Steve B on March 4, 2007, 4:27 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by buffalo on March 4, 2007, 9:34 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Steve B on March 4, 2007, 9:48 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by * on March 5, 2007, 8:17 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Nylon sling question March 3, 2007, 6:22 pm
Follow up harbor freight 1 ton sling December 16, 2006, 6:16 pm
Posting project outcome November 20, 2006, 11:46 pm
Battery charger (outcome) November 26, 2006, 9:28 pm
get your substantially differentiating outcome along my conference August 13, 2007, 12:23 am
OUTCOME -- search for good compressor hose December 26, 2006, 11:24 pm
Outcome -- lubing drill press column March 13, 2007, 9:45 pm
Belt grinder speed followup (project outcome) November 25, 2006, 5:37 pm
osama's outcome amounts in our performance after we chat in connection with it August 13, 2007, 1:03 am
Outcome (was 2 "ground rod" questions (Thumper aka cable fault locator)) December 16, 2006, 6:28 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap