Polishing stainless steel Dan_Musicant 10-30-2007
Posted by Dan_Musicant on October 30, 2007, 1:40 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Dan_Musicant on October 30, 2007, 5:50 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Ed Huntress on October 30, 2007, 6:45 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Dan_Musicant on October 30, 2007, 9:21 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Ed Huntress on October 30, 2007, 10:03 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Polishing stainless steel March 25, 2006, 8:48 am
Stainless polishing April 6, 2008, 9:17 am
Stainless steel nuts galling on stainless steel bolts April 9, 2006, 12:24 pm
polishing stainless 2" pipe September 7, 2006, 7:39 pm
Polishing stainless? (Dumb question for the week) October 8, 2006, 9:46 am
Shining stainless steel September 5, 2006, 8:46 pm
Bending 304 stainless steel October 23, 2006, 9:23 am
Bending 4mm dia stainless steel rod December 5, 2006, 11:51 am
Need Help - Stainless Steel Tubing March 20, 2006, 10:45 pm
CONE FROM STAINLESS STEEL March 5, 2008, 7:51 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap