Posted by Andrew VK3BFA on July 12, 2007, 9:11 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Nick Mueller on July 12, 2007, 10:29 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Karl Townsend on July 12, 2007, 11:00 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Gunner on July 12, 2007, 1:01 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by F. George McDuffee on July 12, 2007, 2:19 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Query - fly cutter tol grinding geometry. July 4, 2007, 5:24 am
Re: Query - fly cutter tol grinding geometry. July 5, 2007, 8:32 pm
tool & cutter grinding book August 27, 2006, 7:11 am
Re: Shaper tool geometry July 26, 2006, 8:23 am
Re: Shaper tool geometry July 26, 2006, 2:22 pm
Tolerances for grinding a 43" cutter blade October 27, 2006, 2:04 am
Tool grinding May 3, 2007, 11:46 pm
Tool grinding angles August 7, 2006, 9:00 am
Tool bit for fly cutter (FC) February 10, 2007, 3:57 pm
Grinding M42 tool blanks for use on shaper or lathe December 8, 2006, 9:57 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap