>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Brent on September 23, 2007, 5:07 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Trevor Jones on September 23, 2007, 6:13 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Terry Keeley on September 23, 2007, 6:52 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Wild_Bill on September 25, 2007, 9:54 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
FS: ProtoTrak Knee Mill July 24, 2006, 10:24 pm
WTD: knee mill 40 taper March 4, 2007, 8:06 am
Re: Knee Mill Drawings Needed March 28, 2007, 1:30 am
Where are the knee locks on a Millrite MVI vertical mill? February 4, 2007, 1:28 pm
Flood coolant guard for knee mill June 11, 2008, 3:10 pm
Knee locks on a Millrite MVI vertical mill - resolved February 10, 2007, 4:11 pm
Would you like to learn Chinese Learn Chinese ,chinese instrument and travel in Beijing December 28, 2007, 9:33 pm
Broken knee gib on BP resurrected January 2, 2007, 1:04 am
Another broken Bridgeport knee gib! January 2, 2007, 8:04 am
Who needed the knee hndle for K&T#2? I got one March 24, 2007, 10:04 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap