>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Jim Stewart on September 21, 2007, 12:01 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Be Careful Out There... February 6, 2008, 2:40 pm
Be careful with shotguns July 14, 2006, 11:31 am
Be careful with shotguns - What would you have done? July 17, 2006, 12:18 am
Be careful grinding or using a chop saw. October 22, 2006, 1:59 pm
he'll be dominating in conjunction with careful Ahmed until his bunch joins biweekly August 12, 2007, 8:58 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap