SATIN CHROME FINISH JimInsolo 10-27-2006
Posted by JimInsolo on October 27, 2006, 8:30 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Lloyd E. Sponenburgh on October 27, 2006, 8:33 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by JimInsolo on October 27, 2006, 9:17 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Don Foreman on October 27, 2006, 11:21 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
satin chrome dials? December 22, 2006, 7:48 pm
Satin coat sheet metal March 18, 2006, 8:41 pm
Nickle Chrome prep March 30, 2006, 3:00 pm
solder copper onto chrome pliers May 22, 2007, 5:07 pm
Mirror finish March 21, 2007, 8:52 pm
grinding finish July 11, 2007, 8:56 am
Surface finish and DOC. August 30, 2007, 10:35 am
Non-toxic finish on raw steel October 15, 2006, 3:34 pm
Spray-on aluminum finish? February 18, 2007, 2:44 pm
Finish cuts: how lite? August 9, 2007, 9:53 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap