>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on December 3, 2006, 3:01 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on December 3, 2006, 3:34 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Bill Marrs on December 3, 2006, 4:58 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on December 3, 2006, 5:42 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Where to get small diameter sex bolts October 18, 2006, 12:29 am
OT: Small diameter magnetic roller between wheels to provide frictionless braking resistance? August 29, 2007, 3:11 pm
Feed Rate Question - Small Hole November 8, 2006, 3:01 pm
New fuel guage May 4, 2007, 1:00 pm
Common uses for Starret No. 643 depth guage July 5, 2006, 6:18 pm
Enclosed digital height guage? August 2, 2007, 12:40 pm
Cutting 10 guage plate steel with a Skill saw. March 30, 2007, 1:00 am
Retarding torque on shear back guage motor? January 27, 2007, 8:38 pm
how small a blower/vac for small bead blast cabinet -- micro cyclone? February 26, 2007, 1:19 am
4 inch diameter bolts August 29, 2006, 1:21 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap