>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Hunter on June 30, 2007, 5:22 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by John Doe on June 30, 2007, 6:07 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Anthony on June 30, 2007, 7:27 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by DoN. Nichols on June 30, 2007, 7:22 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Fancy wire rope ends? September 8, 2008, 10:58 pm
Device to measure axial forces on lathe ? September 19, 2008, 7:53 am
Torsion springs question July 19, 2006, 6:54 am
Can springs be permanently stretched? February 5, 2007, 7:50 am
Source for Springs required March 18, 2006, 8:29 pm
Shop press springs??? April 1, 2006, 8:34 pm
De-arching leaf springs ? March 18, 2008, 5:48 pm
Sulphur Springs Steam April 15, 2008, 4:06 pm
Introducing The Hz2.1 Portable Hot Stamp Wire Marker to Meet Industry's Need for Flexible, Cost-effective Wire Marking April 30, 2007, 4:13 pm
How to Measure Strength of Small Springs? January 11, 2008, 7:01 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap