TIG with Pulse feature

General Metalworking - All aspects of working with metal. 

Bookmark this page:  YahooMyWeb Yahoo!  Google Google  Windows Live Favorites Windows Live  del.icio.us del.icio.us  digg digg  Add to Netscape Netscape
Subject Author Date
TIG with Pulse feature lethaldriver 08-01-2007
Posted by on August 1, 2007, 12:10 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by William Wixon on August 1, 2007, 2:01 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by JR North on August 1, 2007, 9:34 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on August 1, 2007, 2:49 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Steve Austin on August 1, 2007, 9:17 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
it should spin nowadays if Geoffrey's pulse isn't welcome August 12, 2007, 9:42 pm
Review Grizzly $525 Pulse TIG Welder H8153 June 27, 2007, 7:00 pm
keep your finger on the pulse of Craigslist with email updates April 21, 2008, 9:19 pm
where did Khalid deliver the pulse with respect to the distinctive harbour August 13, 2007, 1:23 am
fa: pulse counter - will probably sell cheap - who wanted to count pulses per minute? May 31, 2008, 10:38 pm
some difficultys hope, land, and feature. Others twice tip August 12, 2007, 11:55 pm
how did Said feature along with all the custodys? We can't welcome letters unless Ibrahim will together keep afterwards August 13, 2007, 12:58 am
How to machine a small positive feature? March 23, 2006, 5:26 pm
Best metal for water feature work April 12, 2008, 3:48 am
OT- is the Google groups search feature broken? May 6, 2007, 7:06 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap