Twisting 2" square tube and 1" square steel

General Metalworking - All aspects of working with metal. 

Bookmark this page:  YahooMyWeb Yahoo!  Google Google  Windows Live Favorites Windows Live  del.icio.us del.icio.us  digg digg  Add to Netscape Netscape
Subject Author Date
Twisting 2" square tube and 1" square steel pccruiser 12-26-2006
Posted by pccruiser on December 26, 2006, 1:22 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Pete C. on December 26, 2006, 1:32 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Grant Erwin on December 26, 2006, 1:44 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Steve B on December 26, 2006, 7:53 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Gerald Miller on December 27, 2006, 1:33 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
painting inside of square steel tube July 16, 2007, 5:17 pm
90 Degree joints, square tube steel April 20, 2006, 12:42 am
Slotting Square Tube March 20, 2006, 9:26 pm
internal debur of square tube? October 11, 2006, 7:23 pm
DOM Square Tube - Twist and Straightness November 7, 2007, 5:26 pm
How to drill series of holes in square tube. December 31, 2006, 3:56 pm
Revisiting: multiple holes in square aluminum tube October 6, 2006, 8:04 pm
Re: Strength of materials question: square tube vs angle iron April 14, 2008, 11:25 am
Re: Strength of materials question: square tube vs angle iron April 14, 2008, 11:44 am
Re: Strength of materials question: square tube vs angle iron April 15, 2008, 12:55 am