>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Gerry on January 19, 2008, 7:51 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Christopher Tidy on January 19, 2008, 8:04 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Harold and Susan Vordos on January 19, 2008, 11:07 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Carl Boyd on January 20, 2008, 1:46 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
OT: Plating January 15, 2007, 10:18 pm
Plating removal September 29, 2006, 12:56 am
Gold plating car emblems March 31, 2006, 2:34 pm
Plating SS Screws with brass April 9, 2008, 6:36 pm
Re: A little plating and anodizing current regulator March 14, 2006, 12:41 am
Re: A little plating and anodizing current regulator March 14, 2006, 2:20 am
$200 For Short Phone Interview Of Metal Plating Expert April 8, 2007, 8:56 pm
Electro Plating silver gold nickel vintage manual 1918 FA May 6, 2006, 11:05 am
Electro Plating silver gold nickel vintage manual 1918 FA April 30, 2006, 7:20 pm
What's the right name for a kind of box wrench July 29, 2006, 12:08 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap