>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by PeterM on June 2, 2007, 9:32 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Jon Elson on June 3, 2007, 1:35 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by PeterM on June 3, 2007, 9:26 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Dick on June 5, 2007, 2:31 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Anyone heard about Aircraft Machine Corp Milling machines? September 29, 2006, 3:12 pm
Ballpark of the weight of a milling machine head and how to separate the head form the machine safely June 19, 2007, 5:43 pm
mounting milling machine August 16, 2006, 9:37 am
FS: No.4 Cincinatti milling machine October 26, 2006, 10:09 pm
Milling Machine on casters? March 9, 2007, 9:20 am
Very interesting milling machine August 9, 2007, 12:10 pm
Milling machine up for auction. September 12, 2007, 9:10 pm
FS - Milling machine, Lowell, MA January 14, 2008, 11:31 am
Milling Machine vibration October 14, 2008, 9:56 pm
Atlas Milling Machine Indexer? August 5, 2006, 11:21 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap