Posted by Sam on July 26, 2007, 11:31 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Todd Rich on July 26, 2007, 11:56 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by RoyJ on July 26, 2007, 11:58 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Todd Rich on July 26, 2007, 12:23 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Miller Gold star 300ss July 25, 2007, 5:56 pm
Determining gold plate and solid gold for refining. November 20, 2006, 12:31 pm
Star mill February 2, 2007, 6:13 pm
Re: star trek communicator August 3, 2008, 3:56 am
Re: star trek communicator August 3, 2008, 6:56 am
Opinions? North Star Generators.. March 2, 2007, 4:23 pm
Unique Need for Torx/Star bits. December 27, 2007, 7:08 pm
they are puting in support of the star now, won't criticize jars later August 12, 2007, 11:25 pm
seneca falls star lathe update, redrive April 11, 2006, 12:06 am
Armani ED Hardy Sneakers Coach bag&Shoes, G-star Helen Bape Cheap Wholesale December 15, 2007, 9:50 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap