removing powder coating? Grant Erwin 10-09-2006
Posted by Carl Byrns on October 9, 2006, 11:49 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Tom Stovall on October 9, 2006, 10:11 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Richard J Kinch on October 9, 2006, 10:23 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by axolotl on October 9, 2006, 10:49 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Gunner on October 10, 2006, 5:34 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
DIY powder coating? February 9, 2007, 1:40 pm
HF powder coating system November 12, 2006, 8:58 pm
Anyone know a place I can get powder coating done near Central OH? October 27, 2006, 4:57 pm
feedback on Sears Craftsman powder coating gun? May 3, 2006, 1:40 pm
How to fill pitted aluminum for powder coating? April 1, 2006, 1:45 am
silicon metal powder October 8, 2006, 9:38 pm
silicon metal powder October 12, 2006, 8:26 pm
OT: sensor for a powder balance November 18, 2007, 11:10 am
What is the powder inside power leads ? January 5, 2007, 9:46 pm
Source for aluminum powder in toronto December 21, 2007, 10:03 am

Contact Us | Privacy Policy

XML SitemapXML Sitemap