>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by =?ISO-8859-1?Q?Nick_M=FCller?= on October 3, 2006, 12:06 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by RoyJ on October 3, 2006, 12:33 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by on October 4, 2006, 3:05 am
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Tom Stovall on October 4, 2006, 9:51 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
Re: Tapping aluminum (or tapping on wood?) December 15, 2007, 9:13 pm
Re: Tapping aluminum (or tapping on wood?) December 15, 2007, 10:35 pm
Re: Tapping aluminum (or tapping on wood?) December 17, 2007, 1:17 am
Looks like punched hole? January 28, 2007, 3:38 pm
Punched a hole in my gas tank last night January 10, 2008, 1:51 pm
how many holes should I get out of this end mill? January 1, 2007, 3:23 am
Pressure and three holes April 5, 2007, 9:39 pm
Tapping gun questions January 26, 2007, 7:07 am
Tapping questions March 20, 2007, 12:43 pm
Cleanup after tapping AL October 16, 2007, 10:13 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap