>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Ignoramus16400 on October 30, 2006, 10:47 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Snag on October 30, 2006, 11:10 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Cydrome Leader on October 31, 2006, 7:44 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Posted by Ken Davey on November 11, 2006, 3:47 pm
Please log in for more thread options

>I will give that a try if I can't find the ammonium version. I have some
>pipe flux with zinc chloride but it is only 8%.
>
> --
> Glenn Ashmore


Don't forget, you can make your own (much stronger) by killing some
hydrochloric acid with a handful of zinc. (I presume you have zinc lying
around if you're galvanising stuff.) Otherwise use scrap galvanised steel.

Cheers
--
Jeff R.




Similar ThreadsPosted
shank adapter, extension rod, button bit, thread bit,taper bit, taper rod, drill rod, drill bit, corss bit, chisel bit, DTH hammer drilling ,rock drill, drill tube, casing shoe, drilling tool, core bit, core barrel, ODEX, TUBEX, quarrying,mining equipment September 8, 2006, 2:22 am
Re: Another 4-start thread question - 1/4" internal thread April 2, 2006, 5:25 pm
class of thread fit on studs and all-thread January 23, 2007, 10:18 am
CO2 adapter? July 12, 2006, 1:01 am
"Adapter" for compactflash July 14, 2007, 1:28 am
Re: Special Adapter... December 12, 2007, 3:07 pm
Re: Special Adapter... December 13, 2007, 10:10 pm
J33 to MT2 Adapter - Strange One April 3, 2006, 12:20 pm
Adapter plate December 25, 2008, 9:10 pm
I need a special adapter for a drill June 22, 2007, 12:50 pm

Contact Us | Privacy Policy

XML SitemapXML Sitemap